Skip to main content
. 2019 May 9;6(2):41. doi: 10.3390/bioengineering6020041

Table 2.

The summary of all measurements performed on the PMMA samples and cells, including the average diameter of fiber (Df), average roughness (Ra), the average distance between fibers (Sf), and the water contact angle (θ), on all PMMA surfaces; and the filopodia length, after 3 days of cell culture (Lc).

Scaffold/Film Df [µm] Sf [µm] Ra [µm] θ [⁰] Lc [µm]
Nanofibers 0.34 ± 0.10 0.59 ± 0.33 1.20 ± 0.18 116.0 ± 4.2 0.47 ± 0.21
Microfibers 3.59 ± 0.44 3.21 ± 1.98 7.03 ± 0.30 139.9 ± 3.3 12.96 ± 6.78
Ribbons 3.93 ± 1.37 * - 0.70 ± 0.12 126.9 ± 2.4 -
Films - - 0.26 ± 0.07 70.0 ± 1.9 -

* In case of ribbons, the width of the fiber was measured.