Cold crystallization and melting thermographs of neat and hybrid composites: effect of filler loading at heating rates of (a) 5 °C/min, (b) 10 °C/min, and (c) 20 °C/min; effect of filler treatment at heating rates of (d) 5 °C/min, (e) 10 °C/min, and (f) 20 °C/min.