Skip to main content
. 2019 Jun 14;12(12):1921. doi: 10.3390/ma12121921

Table 1.

Distribution of failure modes among the experimental subgroups: adhesive failure occurs at the dentin–material interface, cohesive failure occurs within the material, and mixed failure is a combination of the two failure modes.

Failure Mode Cohesive of 10 Adhesive of 10 Mixed of 10 p-Value
Subgroups
Putty 5.25 % Sodium Hypochlorite 1 (10%) 4 (40%) 5 (50%) 0.150
Putty 2% Chlorhexidine Gluconate 3 (30%) 2 (20%) 5 (50%) 0.150
Putty Saline 2 (20%) 6 (60%) 2 (20%) 0.905
Paste 5.25 % Sodium Hypochlorite 1 (10%) 1 (10%) 8 (80%) 0.007
Paste 2% Chlorhexidine Gluconate 6 (60%) 0 (0%) 4 (40%) 0.007
Paste Saline 3(30%) 1(10%) 6 (60%) 0.000