. 2019 Jun 3;11(6):965. doi: 10.3390/polym11060965

Figure 4.

Figure 4

Hydrophilicity and degradation behavior of PEGS elastomers. (A) Contact angle of PEGS elastomers. (B) In vitro and in vivo degradation of PEGS elastomers. Asterisks indicate significant differences, * p < 0.05, ** p < 0.01.