Table 1.
Raw | Recycled | |
---|---|---|
Density (g/cm3) | 1.22 | 1.25 |
Vicat B °C 10 N (50 °C/h) | 90 | 94 |
HDT °C 1.82 MN/m² ISO 75 242 °C |
70 | 74 |
Molding shrinkage % ISO 294-4 |
1.35 | 1.15 |
Ejection temperature (°C) | 110 | 118 |
Raw | Recycled | |
---|---|---|
Density (g/cm3) | 1.22 | 1.25 |
Vicat B °C 10 N (50 °C/h) | 90 | 94 |
HDT °C 1.82 MN/m² ISO 75 242 °C |
70 | 74 |
Molding shrinkage % ISO 294-4 |
1.35 | 1.15 |
Ejection temperature (°C) | 110 | 118 |