Electrical conductivity (S/cm) for side-by-side and blends.

PEO-PANI Blend Side-by-Side
3%–1.5% 6.8–9.2 × 10-6 5.817.9 × 10−5
3%–2.5% 2.5–4.3 × 10-5 1.6–3.8 × 10−4
3%–3.5% 2.8–4.3 × 10-5 3.5–5.8 × 10−4
4%–1.5% 1.4–2.6 × 10-6 2.1–3.7 × 10−5
4%–2.5% 1.3–2.5 × 10-5 0.8–1.5 × 10−4
4%–3.5% 2.1–3.6 × 10-5 2.6–5.2 × 10−4
5%–1.5% Not Spinnable 1.3–3.2 × 10−6
5%–2.5% 0.9–1.4 × 10−4
5%–3.5% 1.3–1.9 × 10−4