Table 4.

The concentrations of the tested silver(I) cyanoximates embedded into polymeric composite that inhibited biofilm growth. The lowest inhibiting concentrations (0.5%) are shown in bold. Chlorhexidine was used as a reference compound.

BIOFILM S. aureus B. aryabhattai PAO1 FRD1
Ag(ECO) 1% 5% 1% 0.5%
Ag(ACO) 1% 2.5% 2.5% 2.5%
Ag(BCO) 5% 2.5% 5% 2.5%
Ag(CCO) 5% >5% 2.5% >5%
Ag(BOCO) 1% >5% 0.5% 2.5%
Ag(BIMCO) 5% 2.5% 1% 0.5%
Ag(BIHCO) 0.5% 5% >5% 0.5%
Ag(PiCO) yellow 2.5% 2.5% 0.5% 0.5%
Ag(PiCO) red 2.5% 2.5% 1% 1%
Ag(BTCO) 5% 0.5% 2.5% 2.5%
Ag(MCO) 5% 1% 1% >5%
Ag(PiPCO) 2.5% 2.5% 1% >5%
Chlorhexidine 0.5% 0.5% >5% 2.5%