Skip to main content
. 2019 Jun 1;11(6):952. doi: 10.3390/polym11060952

Figure 4.

Figure 4

The strain amplitude sweep test of P(AAc-co-Am)/PVA double network hydrogels at a fixed angular frequency (10 rad/s) at 37 °C: (a) hydrogels with various Am/AAc ratios; (b) hydrogels with various Fe3+ concentrations.