Figure 3.

Figure 3

(a) Photos of the ECAs filled silver nanowires with 20, 30, and 40 wt% loadings. (b,c) The variations in resistance of ECAs filled silver nanowires with different loadings during curing at room temperature for 7 h: (b) 20 wt%, (c) 30 and 40 wt%. The inset in Figure 3b shows the locally magnified curve.