Skip to main content
. 2017 Feb 23;2(2):653–662. doi: 10.1021/acsomega.7b00043

Table 2. Magnetic Properties of the As-Spun and Dealloyed Ribbons before and after the Fenton Reaction.

material saturation magnetization Ms, emu g–1 remanence Mr, emu g–1 coercivity Hc, Oe
polished as-spun ribbon before Fenton 73.1 7.2 317.3
dealloyed ribbon before Fenton 99.3 8.5 349.6
as-spun ribbon after Fenton reaction ∼0.87 ∼0.06 197.5
dealloyed ribbon after Fenton reaction ∼0.31 ∼0.03 268.8