. 2017 Jun 16;2(6):2678–2688. doi: 10.1021/acsomega.7b00387

Figure 6.

Figure 6

Typical SEM images of the tensile fracture cross-section of (a) PLA, (b) PLA5CNC, (c) PLAIm-PLLA, (d) PLAIm-PLLA+10CNC, (e) PLAPEG-b-PLLA, and (f) PLAPEG-b-PLLA+10CNC.