Table 1. Thermal Data of PS Adducts.

  DSC heating
DSC cooling
TGA
  Tg/°C aTrecrys/°C ΔHrecrys (J g–1) Tmelt/°C ΔHmelt (J g–1) Tsolid/°C ΔHsolid (J g–1) Tonset/°C bTmax (°C) cresidue/%
POSS–PS –4.2             323.4 338.8, 465.2 4.3
VEIm–PS 22.2 42.7, 79.9 17.52, 7.39 124.5 –79.99 98.0 28.36 272.4 313.6 0.9
MDIm–PS   113.7 10.97 132.0 –62.58 114.0 55.06 308.7 395.1 0.9
VDIm–PS       120.9, 135.7 –26.75, −10.20 104.8 47.59 278.5 319.4 9.3
a

Trecrys: temperature of recrystallization (Tonset).

b

Tmax: temperature of the maximum rate of degradation.

c

Residue at 800 °C under N2 flow at 10 °C min–1.