Table 1. BET Surface Area and DFT Pore Volume of the Carbons Derived from LDPE-C and HDPE-C.
sample | BET surface area (m2/g) | DFT pore volume (cm3/g) | mean pore width (nm) |
---|---|---|---|
LDPE-C | 752.3 | 0.33 | 1.13 |
HDPE-C | 673.5 | 0.37 | 1.13 |
sample | BET surface area (m2/g) | DFT pore volume (cm3/g) | mean pore width (nm) |
---|---|---|---|
LDPE-C | 752.3 | 0.33 | 1.13 |
HDPE-C | 673.5 | 0.37 | 1.13 |