Surface excess (ΓSPR) of XG versus cellulose film thickness (d) for XG adsorbed onto RC (■, ——), s-CNC (▲, — · ·), and d-CNC (●, ---) films after 2 h of exposure to a 100 mg·L–1 XG solution. Average-value trend lines are provided as a guide to the eye.