Skip to main content
. 2018 Jul 13;3(7):7846–7855. doi: 10.1021/acsomega.8b00765

Figure 7.

Figure 7

(a) 3D representations of 10 cycling scans for MB degradation by NiO@PANI/RGO, (b) variation in the degradation efficiency of the ternary catalyst during 10 degradation cycles, and (c) XRD profile of NiO@PANI/RGO, before and after the degradation cycle.