(a) Distribution of hydrodynamic diameters of PNIPAM (wp = 0.015 wt %, D2O) with t-BuAM, t-BuOH, t-BuME, or t-BuMK (wadditive = 5 wt % for all additives) measured at 50 °C. (b) Plot of average values of hydrodynamic diameters.