Table 1. Cell Parameters of the H2O2-PFCs under Illumination of Simulated Sunlight (AM 1.5, 100 mW cm–2, 1 sun).

photoanode N Voc (V) Jsc (mA cm–2) Jmax (mA cm–2) Pmax (mW cm–2)
ms-BiVO4 1 0.59 0.068 0.034 0.0092
ms-BiVO4 3 0.54 0.61 0.26 0.075
ms-BiVO4 5 0.58 0.67 0.37 0.11
ms-BiVO4 7 0.59 0.79 0.44 0.13
ms-BiVO4 10 0.61 0.81 0.46 0.13
ms-BiVO4 15 0.61 0.58 0.29 0.09
mp-TiO2 a 0.31 0.01 0.007 0.0015
a

The thickness of mp-TiO2 film was ∼4 μm.