Table 1. Cell Parameters of the H2O2-PFCs under Illumination of Simulated Sunlight (AM 1.5, 100 mW cm–2, 1 sun).
photoanode | N | Voc (V) | Jsc (mA cm–2) | Jmax (mA cm–2) | Pmax (mW cm–2) |
---|---|---|---|---|---|
ms-BiVO4 | 1 | 0.59 | 0.068 | 0.034 | 0.0092 |
ms-BiVO4 | 3 | 0.54 | 0.61 | 0.26 | 0.075 |
ms-BiVO4 | 5 | 0.58 | 0.67 | 0.37 | 0.11 |
ms-BiVO4 | 7 | 0.59 | 0.79 | 0.44 | 0.13 |
ms-BiVO4 | 10 | 0.61 | 0.81 | 0.46 | 0.13 |
ms-BiVO4 | 15 | 0.61 | 0.58 | 0.29 | 0.09 |
mp-TiO2 | a | 0.31 | 0.01 | 0.007 | 0.0015 |
The thickness of mp-TiO2 film was ∼4 μm.