Figure 7.
Comparison of PDH selectivity performed at 550 °C, propane (3% in Ar) flow rate is 20 mL/min, using Co/SiO2 and Co–Zr/SiO2 with increasing Zr loading (numbers indicate molar ratio of Co to Zr).
Comparison of PDH selectivity performed at 550 °C, propane (3% in Ar) flow rate is 20 mL/min, using Co/SiO2 and Co–Zr/SiO2 with increasing Zr loading (numbers indicate molar ratio of Co to Zr).