Skip to main content
. 2017 Nov 16;2(11):8039–8050. doi: 10.1021/acsomega.7b01275

Figure 8.

Figure 8

(a) C′(ω) vs frequency and (b) C″(ω) vs frequency of OFG wherein the electrodes were prepared with different binders in the EG solvent for OFG dispersion. The electrodes were dried at 170 °C.