Skip to main content
. 2019 Apr 25;47(8):1725–1737. doi: 10.1007/s10439-019-02267-4

Figure 6.

Figure 6

(a) LEDs in condition 2 experience total fracture after experimental impacts. (b) Principal stress distribution of the back of the LED for condition 2 in the original configuration. High stress concentration can be observed at the interface of the LED and the dental model. A maximum principal stress of 1176 MPa was observed at 0.79 ms.