Skip to main content
. 2019 Mar 5;4(3):4832–4838. doi: 10.1021/acsomega.8b03566

Figure 3.

Figure 3

SEM micrographs of degummed silkworm fibers from each group at 2500× magnification (left) and 7500× magnification (right). (A,B) Control silkworm fibers. (C,D) LGS-treated silkworm fibers. (E,F) GR–0.2LGS-treated silkworm fibers. (G,H) GR–1LGS-treated silkworm fibers. (I,J) SWNT–0.2LGS-treated silkworm fibers. (K,L) SWNT–1LGS-treated silkworm fibers. Scale bars = 20 and 5 μm for 2500× and 7500×, respectively.