Figure 2.

Figure 2

(A, A′) TEM images of Cu0–AuNPs (panel A) and L1@Cu2+–AuNPs (panel A′). (B) Normalized UV–vis absorption and scale bars: 50 and 20 nm for Cu–AuNPs and 0.2 μm and 100 nm for L1@Cu2+–AuNPs and CuCl2·6H2O as control. (C) Raman spectra of Cu–AuNPs and L1@Cu2+–AuNPs products compared to free L1 and CuCl2·6H2O as control. Raman spectra. Experimental conditions: λexc = 785 nm; laser power 20 mW; accumulation time 180 s.