Figure 1.

Figure 1

Preparation of the NR films by solvent casting. The films were left to dry after casting under normal atmosphere (a). Thereafter, they were rolled (b) into cylinders (c) and finally vulcanized into 50 × 10 mm sheets from the rolled probes (d).