Skip to main content
. 2019 Feb 28;4(2):4448–4460. doi: 10.1021/acsomega.8b03369

Figure 11.

Figure 11

TEM images of the pure carbon materials treated at 800 °C (top) and the iron oxide-loaded composites pyrolyzed at 500 °C (middle) and 800 °C (bottom).