Table 1. Relative Mass Losses per Temperature Step (100 °C) of the Pure and Iron Oxide-Loaded Hydrochar during Sequential TPD Measurements in He in a Thermobalance.
sample | mass loss [wt %] | sample | mass loss [wt %] |
---|---|---|---|
HTC-0 | FeHTC-0 | ||
HTC-200 | 4 | FeHTC-200 | 5 |
HTC-300 | 12 | FeHTC-300 | 21 |
HTC-400 | 16 | FeHTC-400 | 15 |
HTC-500 | 9 | FeHTC-500 | 7 |
HTC-600 | 5 | FeHTC-600 | 6 |
HTC-700 | 3 | FeHTC-700 | 2 |
HTC-800 | 1 | FeHTC-800 | 1 |