Skip to main content
. 2019 Jan 2;4(1):95–103. doi: 10.1021/acsomega.8b02255

Figure 3.

Figure 3

Porosities of the precursor membranes (top half) and cross-linked membranes (bottom half) of CPE-1, CPE-2, CPE-3, CPE-4, and CPE-5 under heat treatment at different temperatures from 120 to 300 °C.