Figure 2.

Figure 2

SEM images of fracture surfaces of specimens from the VT23M alloy at various magnifications: (a)—x3000; (b)—x1200; (c)—x800; (d)—x200; a frame on the fracture surface provides a link to the location of the fragment of the fracture surface shown in Figure 2a.