Skip to main content
. Author manuscript; available in PMC: 2019 Jul 29.
Published in final edited form as: J Biomed Mater Res A. 2017 Mar 27;105(6):1618–1623. doi: 10.1002/jbm.a.35973

Figure 1:

Figure 1:

(A) Solvent swelling ratios of cured PGD, (B) tangent moduli measured at 12.5% strain at 37°C (medium and high cured PGD) or 44°C (low cured PGD), and (C) elastic moduli measured at 21°C. *p ≤ 0.05, ***p ≤ 0.001.