Studies on the reduction of 4-NP using various catalysts.

Catalyst kapp (s−1) Activity Factor, K (s−1 mg−1) Reference
CuNWs (0.1 pg) 0.076 7.6 × 108 This study
Cu@MnO2 0.01142 0.571 [12]
CuNPs (12.5 mg) 0.0016 0.00013 [17]
CuNWs 0.0042 0.046 [21]
CuNW–Ag 0.0067 0.074 [21]
CuCubes (9.5 nm) 0.0101 0.105 [22]
CuNanoplate 0.0095 0.136 [46]
Porous Cu microsphere 0.0043 0.072 [47]