Skip to main content
. 2019 Jul 22;12(14):2331. doi: 10.3390/ma12142331

Figure 14.

Figure 14

XRD spectrum of Ti6Al4V alloy DMLS: (a) as-build, (b) annealing at 650 °C, (c) annealed at 750 °C, (d) 850 °C, and (e) 950 °C for 2 h, cooled with a furnace.