Skip to main content
. 2019 Jul 21;12(14):2323. doi: 10.3390/ma12142323

Figure 5.

Figure 5

Elongation at break (a), tensile strength (b), and Young’s modulus (c) of the dried BC and NR–BC films modified by the immersion in NRL of various concentrations (0%–10% DRC) at various immersion temperatures.