Table 1.
The parameters utilized for electrospinning. PET—polyethylene terephthalate.
Sample | Output 1 (kV) | Output 2 (kV) | Heat (KW) | Humidity (%) | Temperature (°C) | Feed Rate (mL/h) |
---|---|---|---|---|---|---|
PET_2.5_ctrl | −5.73 | 17.53 | 0.6 | 35 | 27 | 2.5 |
PET_5_ctrl | 5 | |||||
PET_7.5_ctrl | 7.5 | |||||
PET_10_ctrl | 10 |