. 2019 Jul 19;11(7):1204. doi: 10.3390/polym11071204

Table 6.

Tensile properties of polypropylene (PP) and PP-TiO2/CNT (carbon nanotubes) nanocomposites.

Sample Xc Tensile Strength (MPa) Nominal Strain at Break (%) Young’s Modulus (MPa)
PP 56.36 23.93 ± 0.12 53.37 971.57 ± 29.1
PP-TiO2/CNT-1 54.97 23.93 ± 0.19 45.78 894.98 ± 27.1
PP-TiO2/CNT-5 53.56 23.32 ± 0.08 33.24 961.28 ± 31.0
PP-TiO2/CNT-10 52.20 22.75 ± 0.37 22.28 1077.44 ± 26.2