Skip to main content
. 2019 Jul 17;24(14):2605. doi: 10.3390/molecules24142605

Figure 4.

Figure 4

Frequency-dependent reflection loss (RL) curves of S1, S2, S3, and S4 at the thickness of 5 mm.