SEM images of PLA/PBS blends at different PBS contents (a) 10 wt%, (b) 20 wt%, (c) 30 wt%, and (d) 40 wt% with particle diameters from 0.2 to 6.5 µm [35]. Reprinted by permission from Springer Nature: Polymer Bulletin, Accelerated hydrolytic degradation of poly(lactic acid) achieved by adding poly(butylene succinate), Wang, Y.-P.; Xiao, Y.-J.; Duan, J.; Yang, J.-H.; Wang, Y.; Zhang, C.-L., Copyright © Springer-Verlag Berlin Heidelberg 2015.