Table 2.
Sample | RPET Content (wt%) | LPET Content (wt%) | Reinforcing Layer | Employment of Hot Press |
---|---|---|---|---|
P9 | 90 | 10 | - | N |
P7 | 70 | 30 | - | N |
P5 | 50 | 50 | - | N |
HP9 | 90 | 10 | - | Y |
HP7 | 70 | 30 | - | Y |
HP5 | 50 | 50 | - | Y |
HP9C | 90 | 10 | Carbon | Y |
HP7C | 70 | 30 | Carbon | Y |
HP5C | 50 | 50 | Carbon | Y |
HP9B | 90 | 10 | Basalt | Y |
HP7B | 70 | 30 | Basalt | Y |
HP5B | 50 | 50 | Basalt | Y |
HP9K | 90 | 10 | Kevlar | Y |
HP7K | 70 | 30 | Kevlar | Y |
HP5K | 50 | 50 | Kevlar | Y |
LMPET Bonding Layer | - | 100 | - | - |