Table 3. Swelling Properties of the UV-Cured C-PUA/HEMA Resins.

samples water ethanol acetone toluene
C-PUA 0.2 ± 0.1 3.8 ± 1.4 5.4 ± 0.2 9.3 ± 1.3
C-PUA/10%HEMA 0.9 ± 0.1 3.3 ± 0.6 7.5 ± 0.8 5.7 ± 1.1
C-PUA/20%HEMA 0.7 ± 0.1 2.9 ± 0.6 8.9 ± 1.1 5.2 ± 1.7
C-PUA/30%HEMA 0.7 ± 0.1 2.6 ± 0.9 8.8 ± 1.3 2.5 ± 0.6
C-PUA/40%HEMA 1.5 ± 0.2 2.7 ± 0.1 6.6 ± 0.1 2.9 ± 0.5