Material Particle size (μm) Processing route % porosity Average pore size (μm)
CpTi [18] < 45 SLM 65 600
Ti64 [19] 45–100 SEBM 61 450
Ti64 [22] 45–150 LENS™ 23–32 60–700
CpTi [23] 50–150 LENS™ 27 450
Ta [20] 10–25 SLM 80 500
Ta [9,24] 45–75 LENS™ 27–45 200–500