2003 |
Li5La3M2O12 (M = Nb, Ta)-PEO-LiPF6
|
10−6 (25°C) |
Ratner et al., 2000
|
2015 |
Li7La3Zr2O12(LLZO)-PEO-LiClO4
|
4.42 × 10−4 (55°C) |
Shi et al., 2017
|
2015 |
Li0.33La0.557TiO3(LLTO) random nanowire-PAN-LiClO4
|
2.4 × 10−4 (25°C) |
Subianto et al., 2009
|
2015 |
Li2.5Al0.5Ge1.5(PO4)3 (LAGP)-PEO-LiClO4
|
2.6 × 10−4 (55°C) |
Tikekar et al., 2016
|
2015 |
Li7La3Zr2O12(LLZO)-PEO-LiClO4
|
4.42 × 10−4 (55°C) |
Shi et al., 2017
|
2016 |
Li6.4La3Zr2Al0.2O12(LLZO)-PEO-LiTFSI |
2.5 × 10−4 (25°C) |
Stavila et al., 2014
|
2016 |
Li1.5Al0.5Ge1.5(PO4)3 (LAGP)-PEO-LiTFSI |
6.76 × 10−4 (60°C) |
Thokchom et al., 2008
|
2016 |
Li10GeP2S12-PEO-LiTFSI |
10−5 (25°C) |
Verma et al., 2010
|
2017 |
Li6.20Ga0.30La2.95Rb0.05Zr2O12-PVDF-LiTFSI |
1.62 × 10−3 (25°C) |
Scrosati and Garche, 2010
|
2017 |
Li6.75La3Zr1.73Ta0.23O12-PVDF-LiClO4
|
5 × 10−4 (25°C) |
Siqueira and Ribeiro, 2006
|
2017 |
Li0.33La0.557TiO3(LLTO) aligned nanowire-PAN-LiClO4
|
6.05 × 10−5 (30°C) |
Srivastava and Tiwari, 2009
|
2017 |
Li1.3Al0.3Ti1.7(PO4)3(LATP)-PEO-BPEG-LiTFSI |
2.5 × 10−4 (60°C) |
Thangadurai et al., 2003
|
2018 |
Li7La3Zr2O12 (LLZO)-PEO-LiTFSI |
1.12 × 10−4 (25°C) |
Quartarone and Mustarelli, 2011
|
2018 |
Li6.4La3Zr1.4Ta0.6O12(LLZTO)-PEO-LiTFSI |
10−4 (55°C) |
Sheng et al., 2017
|
2018 |
Li0.33La0.557TiO3-PEO-LiClO4
|
2.4 × 10−4 (25°C) |
Stramare et al., 2003
|
2018 |
3D-Li0.35La0.55TiO3(LLTO)-PEO-LiTFSI |
8.8 × 10−5 (25°C) |
Sun et al., 2014
|