Skip to main content
. 2019 Aug 2;12(15):2460. doi: 10.3390/ma12152460

Figure 4.

Figure 4

Hardness of HPT-processed (2 rot) and heat-treated Mg-0.2Zn-0.5Ca. The temperature was 0.45 Tm (142 °C), and the indent direction was equal to ND.