. 2019 Aug 2;12(15):2460. doi: 10.3390/ma12152460

Figure 8.

Figure 8

Hardness of Mg-0.6Zn-0.5Ca in the initial extruded state and after HPT (2 rot) and heat treatment for 1 h.