Skip to main content
. 2019 Jul 27;12(15):2395. doi: 10.3390/ma12152395

Figure 6.

Figure 6

Typical OCP curves of the 18-14, 18-15, and 18-13-1 alloys subjected to TMT and Ti Grade 2 obtained during mechanocycling in Hanks’ solution (1.5% strain, 0.9 Hz).