SEM images of (a) 18-14, (b) 18-13-1, (c) 18-15, and (d) Ti Grade2 fracture surfaces after mechanocycling in Hanks’ solution: (1) fatigue crack initiation area, (2) the crack propagation area, and (3) mechanical rupture area; arrows indicate the crack initiation points [34].