Skip to main content
. 2019 Aug 16;9:11938. doi: 10.1038/s41598-019-48103-6

Figure 5.

Figure 5

Reuse of the ZnO and Ni-W/β catalyst system. Reaction conditions: 30 min, 6 Mpa H2 245 °C, 50 mL of H2O, 0.5 g of cellulose, 0.15 g of catalyst, and 100 mg of ZnO. EG: ethylene glycol; PG: 1,2-propylene glycol; S: sorbitol; and M: mannitol.