Skip to main content
. 2019 Jul 13;6(16):1802286. doi: 10.1002/advs.201802286

Figure 2.

Figure 2

a) Temperature dependent Hall mobility, b) carrier concentration dependent Seebeck coefficient at 300 K, c) room temperature Bi‐alloying dependent Hall mobility and carrier concentration, as well as d) Seebeck coefficient and power factor for Mg3.05Sb2− x yBiy xTex (x ≤ 0.04, y ≤ 1.5) with a comparison to literature results.[qv: 17a,19,20,22a,b] The unit of carrier concentration identifying samples is cm−3.