Skip to main content
. 2019 Aug 22;10:3786. doi: 10.1038/s41467-019-11520-2

Fig. 3.

Fig. 3

SEM image and schematic diagram of the tensile fractures. a CFRP, scale bars 200 μm (left panel), 20 μm (upper right panel) and 50 μm (lower right panel); b HFRP 5C5S-1, scale bars 500 μm (left panel), 100 μm (upper right panel) and 50 μm (lower right panel)