Published in final edited form as: Polymer (Guildf). 2017 Apr 18;117:331–341. doi: 10.1016/j.polymer.2017.04.044

Table 1.

The abbreviations, composition, and geometry of all of the hydrogel samples used in this study. The abbreviations for the groups are meant to emphasize the differences in composition and structure that are being investigated in each experiment. The numbers in bold indicate where the parameters have been changed in each grouping.

Group
Abbreviation
Molecular Weight of PEGDA (Da) Concentration of PEGDA (g/mL of PBS) Concentration of AA (g/mL of PBS) Thickness of Mold for Crosslinking (mm)
100% PEGDA 4000 0.1 0 0.75
1:4 PEGDA:AA 4000 0.1 0.4 0.75
1:8 PEGDA:AA 4000 0.1 0.8 0.75
1:12 PEGDA:AA 4000 0.1 1.2 0.75
1:16 PEGDA:AA 4000 0.1 1.6 0.75
0.9 g/mL 4000 0.1 0.8 0.75
1.8 g/mL 4000 0.2 1.6 0.75
2.7 g/mL 4000 0.3 2.4 0.75
3.6 g/mL 4000 0.4 3.2 0.75
1000 Da 1000 0.1 0.8 0.75
4000 Da 4000 0.1 0.8 0.75
10,000 Da 10,000 0.1 0.8 0.75
0.3 mm 4000 0.1 0.8 0.25
0.7 mm 4000 0.1 0.8 0.5
1.0 mm 4000 0.1 0.8 0.75
1.4 mm 4000 0.1 0.8 1.0
1.7 mm 4000 0.1 0.8 1.25
2.1 mm 4000 0.1 0.8 1.5