Skip to main content
. 2019 Aug 8;12(16):2520. doi: 10.3390/ma12162520

Figure 13.

Figure 13

(a) Representative SEM micrograph of the LDPE-30% vol. glass composite surface after conducting a friction test with the corresponding energy dispersive spectroscopy (EDS) spectra (b) of stacked particles (white arrow). The black arrow indicates a microregion of plastic deformation.