Table 2.

PAni loadings of dried hybrid PAni-ACC composites synthesized after different electropolymerization times.

Time
(min)
Initial Dry Mass
(mg)
Corrected Weight Loss 1
(%)
PAni Weight Loss
(mg)
PAni Total Mass 2
(mg)
PAni Loading
(wt.%) (mg cm−2) 3
10 8.8250 9.12 0.8047 2.2679 25.70 6.23
20 9.2770 7.75 0.7186 2.0251 21.83 5.03
40 9.9108 7.63 0.7561 2.1307 21.50 4.93
60 8.4070 12.58 1.0577 2.9807 35.46 9.89
120 11.1129 17.79 1.9766 5.5704 50.13 18.1

1 After subtraction of the total loss from the carbon fabric support (see text). 2 After considering that a 45 wt.% polymer residue remains on the heat-treated sample. 3 Calculated on the basis of cloth aerial density.